DOW™ Inspire D560.00 Developmental Performance Polymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: D 560.00 Performance Polymer has consistent processability, high gloss, good regrind stability, and contains U.V. stabilizers for increased weatherability. D 560.00 Performance Polymer is intended for use in extrusion blow molding, sheet extrusion, and thermoforming processes where enhanced clarity and weatherability is desired.Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|