DOW™ Inspire 117.00 Performance Polymer
Subcategory: Polypropylene; Thermoplastic
Material Notes: 117.00 Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistance, and clarity are required. It has outstanding heat resistance, excellent balance of high stiffness and toughness, and good contact clarity and gloss, low taste & odor transfer. It contains a nucleating agent and it Complies with U.S. FDA 21 CFR 177.1520.Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|