DOW™ Inspire TF7000 ES Natural Performance Polymer
Subcategory: Elastomer, TPE; Thermoplastic; Polymer
Material Notes: INSPIRE* TF7000 ES Natural Performance Polymer DA™ is a very high stiffness (2400 MPa) TPO designed for instrument panel upper and lower components, as well as other interior trim applications where stiffness, good impact resistance, and good molded-in-color part aesthetics are important. Its high melt flow rate also allows for rapid filling of large parts in the injection molding process. It has excellent surface aesthetics, good scratch & mar resistance, instrument panel uppers/lowers, interior trim applications, high flow, and has been approved on DaimlerChrylser MS-DC265D.Information provided by Dow
| Available Properties |
- Density
- Filler Content
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Yield
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Falling Dart Impact
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, mm/min
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|