Dow Plastics AFFINITY™ GA 1950 Polyolefin Plastomer (POP)
Subcategory: Polyolefin; Thermoplastic
Material Notes: AFFINITY™ GA 1950 Polyolefin Plastomer (POP) is produced via INSITE™ Technology from Dow Plastics. This product can be used in applications such as polymer modification (i.e. flow enhancement and property enhancement), masterbatch / additive carrier, and hot melt adhesives.Information provided by Dow
| Available Properties |
- Density
- Brookfield Viscosity
- Collected Volatile Condensable Material
- Tensile Strength, Ultimate
- Elongation at Break
- Melting Point
- Glass Temperature
- Gardner Color Number
|
|
|
|
| Property Data |