Dow Plastics AFFINITY™ PT 1450G1 Ethylene alpha-olefin resin
Subcategory: Polyolefin; Thermoplastic
Material Notes: AFFINITY™ PT 1450G1 Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. The resin is for monolayer and co-extrusion coating that offers excellent low temperature seal initiation, ultimate seal strength, adhesion to Oriented Polypropylene (OPP) and good taste and odor performance.Information provided by Dow
| Available Properties |
- Density
- Thickness
- Melt Index of Compound
- Neck In
- Coating Weight
- Adhesive Bond Strength
- Heat Seal Strength Initiation Temperarture
- Melting Point
- Vicat Softening Point
- Melt Temperature
|
|
|
|