Dow Plastics AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
Subcategory: Polyolefin; Thermoplastic
Material Notes: AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded industrial and consumer goods and compression molded closure liners or gaskets.Information provided by Dow
| Available Properties |
- Density
- Thickness
- Melt Flow
- Slip Level
- Tensile Strength, Ultimate
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- 2% Secant Modulus
- Izod Impact, Notched
- Vicat Softening Point
- Melt Temperature
|
|
|
|