Dow Plastics AMPLIFY™ VA 400 Ethylene vinyl acetate (EVA)
Subcategory: Thermoplastic
Material Notes: AMPLIFY™ VA 400 Functional Polymer is produced via a high pressure reactor. It exhibits high flexibility, clarity and low temperature sealability. It is easy to process and features functional adhesion to various substrates including polyolefins, cellulose, polyester, polycarbonate, glass, and foil. It provides excellent blend compatibility with polyolefins and fillers.Information provided by Dow
| Available Properties |
- Density
- Filler Content
- Melt Flow
- Hardness, Shore D
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|