Dow Plastics CALIBRE™ 893-20 Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Material Notes: CALIBRE™ 893-20 resin provides superior ignition resistance in opaque applications.
Applications: - Portable/cellular phones
- Pagers
- Data Enclosures
- Computer housings, keyboards
- Structural components
- Business equipment
Information provided by Dow
| Available Properties |
- Specific Gravity
- Water Absorption
- Water Absorption at Saturation
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell M
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Tensile Impact
- Dart Drop, Total Energy
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|