Dow Plastics CONTINUUM™ DGDC-2480 NT Bimodal Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic
Material Notes: CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistance to slow crack growth and rapid crack propagation is desired. Suitable applications include natural gas distribution pipes, industrial piping, mining, sewage, and municipal water service lines. Information provided by Dow
| Available Properties |
- Density
- PENT
- Melt Flow
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Brittleness Temperature
- Resistance to Rapid Crack Propagation, Pc psi
- Resistance to Rapid Crack Propagation, Tc °F
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|