Dow Plastics Dow 722 Low Density Polyethylene (LDPE)
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: Polyethylene 722 is used in flexible packaging and paperboard coating applications such as liquid/juice, laminate tube, condiment pouches, dry foods packaging, snack foods packaging, moist foods packaging, sugar pouches, lidding stock and medical packaging.Information provided by Dow
| Available Properties |
- Density
- Water Vapor Transmission
- Thickness
- Melt Index of Compound
- Neck In
- Coating Weight
- Coefficient of Friction
- Heat Seal Strength Initiation Temperarture
- Melting Point
- Vicat Softening Point
- Melt Temperature
- Line Speed fpm, max
|
|
|
|