Dow Plastics DOW 5E89 Polypropylene Resin
Subcategory: Polypropylene; Thermoplastic
Material Notes: DOW 5E89 is intended for use in stretched tape (raffia) processes, from which the raffia is used to produce woven fabrics for carpet backing, sacking, industrial and geotextile applications.Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |