Dow Plastics DOW C104-01 Polypropylene Resin
Subcategory: Polypropylene; Thermoplastic
Material Notes: DOW C104-01 is intended for use in extrusion and thermoforming applications where impact resistance at refrigeration temperatures is desired. It is especially suited for corrugated board applications.Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |