Dow Plastics DOW DC759.00 Polypropylene Resin
Subcategory: Polypropylene; Thermoplastic
Material Notes: DC759.00 Developmental Polypropylene Resin is an impact copolymer designed for injection molding with high stiffness, relatively good impact resistance, and good antistatic properties. The excellent moldability of this product enables short cycle times.Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Gardner Impact @ -30°C
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|