Dow Plastics DOW DFDC-7525 NT High Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOW DFDC-7525 NT is produced using UNIPOL™ process technology. It is intended for use in thin wall drip tape and micro-irrigation tube, hose and tube, and profile extrusion applications. Information provided by Dow
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|