Dow Plastics DOW DGDB-2480 NT High Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOW DGDA-2475 NT is produced using UNIPOL™ process technology. It is intended for use in pipe applications where long term hydrostatic strength and resistance to slow crack growth are desired. Suitable applications include natural gas distribution pipes, large diameter industrial piping, mining, sewage, and municipal water service lines. Information provided by Dow
| Available Properties |
- Density
- PENT
- Melt Flow
- Melt Index of Compound
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Brittleness Temperature
|
|
|
|