Dow Plastics DOW DMDA-8007 NT 7 High Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin is ideally suited for injection molded crates, cases, trays, tote bins, and other objects requiring high rigidity. Information provided by Dow
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|