Dow Plastics DOW DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: DOW DNDA-7340 NT 7 LLDPE resin is well-suited for use in blow molding applications such as small, squeezable bottles, as well as, extruded flexible hoses and tubing. DOW DMDA-7340 NT 7 resin is also well-suited for use in large blow molded parts, such as drum liners. Additionally, It may also be used in certain sheet and tubing applications. Information provided by Dow
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|