Dow Plastics DOW DNDB-7441 NT 7 Linear Low Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE
Material Notes: DOW DNDB-7441 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in hose and tube applications. It also has utility in gasketing, spiral wound hose, and corrugated hose applications. It is also recommended as a modifier in blends with flexible copolymers such as ethylene ethyl acetate (EVA) and ethylene ethyl acrylate (EAA) to enhance their rigidity in extrusion applications. Information provided by Dow
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Flow
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|