Dow Plastics DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE)
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and peak molecular weight, with a slightly lower density for increased impact strength. Information provided by Dow
| Available Properties |
- Density
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|