Dow Plastics EMERGE™ 5100 Acrylonitrile Butadiene Styrene (ABS)
Subcategory: ABS Polymer; Thermoplastic
Material Notes: EMERGE™ ABS 5100 is a pre-colored, white, ABS resin, having high opacity and excellent toughness intended for manufacture of laser-marketable injection-molded smart cards.Information provided by Dow
| Available Properties |
- Density
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|