Dow Plastics EMERGE™ 8702 Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Material Notes: EMERGE™ PC 8702 advanced resin is an ignition-resistant, 20% glass reinforced, polycarbonate resin. This resin contains no bromide, chloride, or phosphate additives. It is a medium flow PC resin with a mold release system, intended for injection molding applications.
Applications: - Information Technology Equipment
- Electrical Parts
- Other structural/internal parts
Information provided by Dow
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 68°F
- CTE, linear 68°F, Transverse to Flow
- Hot Ball Pressure Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Glow Wire Test
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|