Dow Plastics EMERGE™ 4701-13 Polycarbonate
Subcategory: Polycarbonate; Thermoplastic
Material Notes: EMERGE™ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides superb ignition resistance, rigidity, dimension stability and heat resistance.
Applications: - Information Technology Equipment
- Power Tools
- Electrical Appliances and Parts
Information provided by Dow
| Available Properties |
- Specific Gravity
- Filler Content
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Unnotched
- Izod Impact, Notched
- CTE, linear 68°F
- Hot Ball Pressure Test
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Oxygen Index
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|