Dow Plastics EMERGE™ 4850-19 Polycarbonate

 

Subcategory: Polycarbonate; Thermoplastic

Material Notes:
EMERGE™ 4850-19 advanced resin provides superior ignition resistance and ultraviolet light resistance in opaque applications. It has an f1 rating by Underwriters Laboratories Inc. Physical properties and process-ability are outstanding for this class of polycarbonate resins.

Applications:

  • Consumer Electronics
  • Information Technology Equipment
  • Appliances

Information provided by Dow

Available Properties
  • Specific Gravity
  • Linear Mold Shrinkage
  • Melt Flow
  • Hardness, Rockwell R
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Izod Impact, Unnotched
  • Izod Impact, Notched
  • Comparative Tracking Index
  • CTE, linear 68°F
  • Hot Ball Pressure Test
  • Deflection Temperature at 0.46 MPa (66 psi)
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Vicat Softening Point
  • UL RTI, Electrical
  • UL RTI, Mechanical with Impact
  • UL RTI, Mechanical without Impact
  • Flammability, UL94
  • Oxygen Index
  • Glow Wire Test
  • Melt Temperature
  • Mold Temperature
  • Drying Temperature
  • Dry Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。