Dow Plastics FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube applications as well as for blow molding small squeezable bottles. It has a high molecular weight and a relatively narrow molecular weight distribution and exhibits excellent low temperature toughness and outstanding flex life characteristics. It is also recommended as a blending component to modify and improve the physical properties of high pressure and linear low density polyethylene resins. Information provided by Dow
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 1% Secant Modulus
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|