Dow Plastics FLEXOMER™ ETS-9078 NT 7 Very Low Density Polyethylene (VLDPE) Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: FLEXOMER™ ETS-9078 NT 7 is intended primarily for slot cast extrusion. This narrow molecular weight distribution resin has outstanding drawdown properties and produces low modulus cast films, high clarity and an excellent balance of toughness and stiffness. Information provided by Dow
| Available Properties |
- Density
- Melt Index of Compound
- Melting Point
- Vicat Softening Point
|
|
|
|