Dow Plastics FLEXOMER™ GERS-1088 NT Very Low Density Polyethylene (VLDPE) Resin
Subcategory: Polyethylene; Thermoplastic; LDPE
Material Notes: FLEXOMER™ GERS-1088 NT is an ethylene-butene copolymer produced via gas phase polymerization from Dow. It can be utilized in monolayer and co-extruded films and in blends with other polyolefins to enhance melt strength and toughness of the structure. Granular form enhances rapid melt blending into polypropylene or polyethylene. Information provided by Dow
| Available Properties |
- Density
- Melt Flow
- Melt Index of Compound
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Flexural Modulus
- Melting Point
- Glass Temperature
|
|
|
|