Dow Plastics MAGNUM™ 1150 EM Acrylonitrile Butadiene Styrene (ABS)
Subcategory: ABS Polymer; Thermoplastic
Material Notes: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance, and heat resistance.Information provided by Dow
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Dart Drop, Total Energy
- Falling Dart Impact
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|