Dow Plastics SARAN WRAP™ 3 Plastic Film
Subcategory: PVDC; Thermoplastic; Polymer
Material Notes: SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls, in widths up to 65 inches.Information provided by Dow
| Available Properties |
- Water Vapor Transmission
- Oxygen Transmission
- Nitrogen Transmission
- Carbon Dioxide Transmission
- Thickness
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Heat Seal Strength Initiation Temperarture
- Shrinkage, MD
- Shrinkage, TD
- Haze
- Gloss
- Transmission, Visible
- Air Transmission cc-mil/100 in²-24hr-atm
- Block Force g
- Cling g
- Yield in2/lb
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|