Material Notes: Saran™ 520 Vapor Retarder Tape is a Vapor Retarder Film coated with acrylic adhesive designed for long-lasting adhesion and wide temperature range performance.
Information provided by Dow
Available Properties
Permeability
Thickness
Tensile Strength @ Break
Elongation at Break
Adhesive Bond Strength
Flammability Test
Smoke Density
Property Data