Dow Plastics TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin
Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer
Material Notes:
- Hexene Linear Low Density Resin
- General Purpose Resin
- Excellent Strength
- Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions)
TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, designed for good strength and processability. This product is recommended for general-purpose packaging applications from thick gauge, heavy duty bags to high speed thin gauge applications.Information provided by Dow
| Available Properties |
- Density
- Thickness
- Melt Flow
- Film Tensile Strength at Yield, MD
- Film Tensile Strength at Yield, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Secant Modulus, MD
- Secant Modulus, TD
- Impact
- Impact Test
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Elmendorf Tear Strength, MD
- Elmendorf Tear Strength, TD
- Dart Drop Test
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Heat Seal Strength, Ultimate
- Heat Seal Strength Initiation Temperarture
- Melting Point
- Vicat Softening Point
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|