Dow Plastics TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin

 

Subcategory: Polyethylene; Thermoplastic; LLDPE; Polymer

Material Notes:

  • Hexene Linear Low Density Resin
  • Good Processability at Narrow Die Gaps
  • Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
TUFLIN™ HS-7094 NT 7 is a fractional melt, ethylene-hexene copolymer, designed for good toughness and stiffness. This product is recommended for thin and thick gauge applications such as trash bags and heavy-duty shipping sacks that require strength and output.

Information provided by Dow

Available Properties
  • Density
  • Thickness
  • Melt Flow
  • Antiblock Level
  • Film Tensile Strength at Yield, MD
  • Film Tensile Strength at Yield, TD
  • Film Elongation at Break, MD
  • Film Elongation at Break, TD
  • Secant Modulus, MD
  • Secant Modulus, TD
  • Impact
  • Impact Test
  • Elmendorf Tear Strength MD
  • Elmendorf Tear Strength TD
  • Elmendorf Tear Strength, MD
  • Elmendorf Tear Strength, TD
  • Dart Drop Test
  • Film Tensile Strength at Break, MD
  • Film Tensile Strength at Break, TD
  • Heat Seal Strength, Ultimate
  • Heat Seal Strength Initiation Temperarture
  • Melting Point
  • Vicat Softening Point
  • Haze
  • Gloss
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。