Dow Plastics UNIVAL™ DMDA-6147 NT 7 High Density Polyethylene Resin (HDPE)
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes:
- Good extrudability/processability
- Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDA-6147 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This product provides an excellent combination of extrudability and parison stability, which contribute to uniform wall thickness in large parts. DMDA-6147 NT 7 HDPE resin is ideal for blow molding containers such as the 5-55 gallon closed head shipping containers and other similar parts. The broad distribution also provides outstanding environmental stress crack resistance (ESCR) at a good rigidity. These characteristics mean a wide variety of products, such as industrial chemicals, latex paints, printing inks, foodstuffs, adhesives, and other chemical specialties may be packaged in containers produced from this resin. Information provided by Dow
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|