Dow Plastics UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE)
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes:
- Moderate swell
- Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package household industrial chemicals, toiletries and cosmetics, health and medicinal aids, and food products. In addition it can be blow molded into other thin walled parts and houseware items, and also can be extruded into profiles. Information provided by Dow
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Melt Index of Compound
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|