Dow Plastics UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE)
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes:
- Excellent parison melt strength / low sag
- Good extrudability / process-ability
- Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a
UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distribution and high molecular weight. This product provides good stability, which contributes to uniform wall thickness in large parts, making it ideal for blow molding of containers, such as the 5 - 30 gallon tight-head pails, and other large parts. Information provided by Dow
| Available Properties |
- Density
- ESCR 100% Igepal®
- Melt Flow
- Hardness, Shore D
- Tensile Strength @ Break
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Flexural Modulus
- Tensile Impact Strength
- Melting Point
- Crystallization Temperature
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|