Dow Plastics VORANOL™ RA 800 Polyol
Subcategory: Polyether; Thermoset
Material Notes: VORANOL™ RA 800 polyol is a highly reactive amine initiated polyether polyol, specially developed for the production of rigid polyurethane foams and designed for blending with other polyols.Information provided by Dow
| Available Properties |
- Specific Gravity
- Viscosity Measurement
- Maximum Moisture Content
- Flash Point
- Gardner Color Number
- Basicity meq/g, min
- Hydroxyl Number mg KOH/g
|
|
|
|
| Property Data |