Dow Corning 738 Electrical Sealant
Subcategory: Silicone; Adhesive
Material Notes: Sealant. For bonding and sealing. Can be used in corrosion sensitive electrical and electronic equipment. One part nonslumping RTV paste. Tough, rubbery solid. Cure By-Product: Methanol Listing/Specification: UL, Mil Spec Color(s): White
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Processing Temperature
- Extrusion Rate
- Cure Time
|
|
|
|