Dow Corning 5 Compound
Subcategory: Silicone; Polymer
Material Notes: Compound Features: A dielectric compound used on insulators and bushings; as a lubricant for high-current switches. Nonconductive; water repellent; helps prevent formation of conductive paths; long lasting. Translucent light-gray, heavy-consistency, grease-like silicone paste. Applications: Protective transmission insulators, distribution line insulators, power substation bushings, pole top disconnect switches, insulator threads and bolts, service entrance cable, meters. Base Oil: Silicone Listing/Specification: Color(s): Translucent light gray Thickener: Silica NLGI#: 3
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Penetration
- Penetration P(60), 1/10 mm
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Evaporation
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|