Dow Corning 111 Valve Lubricant & Sealant
Subcategory: Silicone; Polymer; Fluid; Lubricant; Silicone Base
Material Notes: Lubricant Features: General purpose O-ring and valve lubricant. Provides a noncuring moisture barrier; high dielectric strength; moisture and ozone resistance; good thermal, oxidation and chemical stability; suitable fore use with potable water under NSF 61. Heavy consistency, translucent white, grease-like silicone paste. Applications: Lubricating plug, sanitary, gate, ball, butterfly and automate valves, pump packing, rubber and plastic O-rings; sealing vacuum and pressure systems (especially equipment subjected to washing and harsh environments); damping medium for dash pots in electrical equipment. Base Oil: Silicone Listing/Specification: FDA, NSF 51, NSF 61 Color(s): Translucent white Thickener: Silica NLGI#: 3 to 4
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Penetration
- Penetration P(60), 1/10 mm
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Evaporation
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|