Dow Corning 340 Heat Sink Compound
Subcategory: Silicone; Polymer
Material Notes: Compound Features: Thermal coupling of electrical/electronic devices to heat sinks. High thermal conductivity; low bleed; stable at high temperatures. White, grease-like silicone heavily filled with heat-conductive metal oxides. Applications: Applied to the base and mounting studs of transistors, diodes and silicon-controlled rectifiers; thermal coupler for many heat sink devices; high-voltage corona-suppressant; nonflammable coating in flyback transformer connections in TV sets. Base Oil: Silicone Listing/Specification: Color(s): White Thickener: Zinc oxide NLGI#: 2
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Penetration
- Penetration P(60), 1/10 mm
- Dielectric Strength
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Evaporation
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|