Dow Corning 41 High Temp. Bearing Grease
Subcategory: Silicone; Polymer; Fluid; Lubricant
Material Notes: Grease Features: Lubricating ball bearings in high-temperature equipment. Heat stable; resists oxidation, moisture, corrosive atmospheres; moderate loads and speeds. Black, carbon black thickened silicone grease. Applications: Lubricating high-temperature conveyor equipment, plywood drying ovens, industrial ovens and boilers, steam turbine controls, knife-type electric power disconnect switches; power insulator ball-and-socket connections. Base Oil: Silicone Listing/Specification: Color(s): Black Thickener: Carbon black NLGI#: 2
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Saybolt Viscosity at 100°F
- Penetration P(60), 1/10 mm
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Dn Value
- Drop Point
- Evaporation
- Four Ball Wear Scar
- Four Ball Weld Load
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|