Dow Corning 44 O-Ring Lubricant
Subcategory: Silicone; Polymer; Fluid; Lubricant; Synthetic Ether Base; Organic Soap Gellant
Material Notes: Lubricant Features: Lubricating antifriction bearings, plastic and rubber parts under light to moderate loads; designed to give long service life in high-temperature bearings. Resists oxidation, moisture; wide service temperature range; excellent lubricant for plastic components; low to moderate loads; moderate to high speeds. Dark red, lithium soap thickened, silicone grease. Applications: Lubricating motor bearings on appliances, ball bearings in electric motors, kiln preheated fans, one fans, textile slashers and driers, conveyor systems. Base Oil: Silicone Listing/Specification: Color(s): Dark red Thickener: Lithium NLGI#: 1, 2
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Saybolt Viscosity at 100°F
- Penetration P(60), 1/10 mm
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Dn Value
- Drop Point
- Evaporation
- Four Ball Wear Scar
- Four Ball Weld Load
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|