Dow Corning 3451 Chemical Resistant Value Lubricant
Subcategory: Silicone; Polymer; Fluid; Lubricant; Silicone Base
Material Notes: Features: Lubricating bearings exposed to harsh chemical environments, heavy loads or high temperatures. Resists deterioration by chlorides, solvents, fuels, acids and low-pressure steam and condensate; high load-carrying ability; stable at high temperatures, moderate to high loads and speeds. Applications: Lubricating bearings in chemical mixers, pumps, processing equipment, conveyors, fans; sealed-for-life bearings. Base Oil: Fluorosilicone Listing/Specification: USDA Color(s): White Thickener: PTFE NLGI#: 2
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Saybolt Viscosity at 100°F
- Penetration P(60), 1/10 mm
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Dn Value
- Drop Point
- Evaporation
- Four Ball Wear Scar
- Four Ball Weld Load
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|