Dow Corning White E.P. Bearing Grease
Subcategory: Polymer; Fluid; Lubricant; Organic Soap Gellant
Material Notes: Grease Features: Lubricating plain and rolling element bearings in equipment that requires a "clean" grease or that may come in contact with food. "Clean" grease; complies with FDA/USDA regulations for incidental food contact; moderate to high loads and speeds. Applications: Grease-lubricated chains and gears; lubricating good processing equipment, can seamers, filling equipment, rotary kilns. Base Oil: Mineral Listing/Specification: FDA, USDA Color(s): White Thickener: Aluminum complex NLGI#: 2
Data provided by Ellsworth Adhesives.
| Available Properties |
- Density
- Saybolt Viscosity at 100°F
- Penetration P(60), 1/10 mm
- Maximum Service Temperature, Air
- Minimum Service Temperature, Air
- Bleed
- Dn Value
- Drop Point
- Evaporation
- Four Ball Wear Scar
- Four Ball Weld Load
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|