DSM Akulon® K224-HG7 (Dry) 35% Glass Reinforced Nylon 6 (North America)
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Unfilled Extrusion Resins Akulon resins are available with melt viscosities to suit all extrusion processes: barrier and coating film, tube and hose, monofilament, stock shapes. Akulon resins are characterized by: - consistent quality
- high purity
- for film applications, low gel contents.
Molding Resins Suited to all engineering demands: - Unfilled low and medium viscosity grades
- Toughened unfilled grades
- Glass reinforced from 20-45% filled
- Low warpage reinforced grades
- Flame retardant; UL V0 rated and glow wire types
- Halogen free FR grades
- Blow moldable materials
- Laser markable resins
- Laser weldable, high burst pressure grades
- Toughened, reinforced resins
- High stiffness grades for metal replacement
Akulon Ultraflow resins have high flow with mechanical properties similar to standard materials. Exceptional flow allows: - productivity gains in molding
- lower built in stresses
- better surface appearance
- system cost reductions
Applications for Molding resins There is an Akulon resin available suitable for any application requiring polyamides. Key areas where DSM has specific application knowledge are - Automotive
- Under the hood and engine components
- Exterior and interior applications
- Electrical components and connectors
- Electrical
- Low voltage power distribution
- Lighting
- Power connectors
- Consumer Durables
- Power and lawn and garden tools
- Small Appliances
- Sports and leisure equipment
- Furniture accessories
- Industrial Goods
- Transportation (railways)
Information provided by DSM.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Unnotched Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Heat stabilized or stable to heat
- Injection Molding
- Release agent
- With fillers
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|