DSM Akulon® S223-G4U (Cond.) 23% Glass Reinforced Nylon 66 (North America)

 

Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer

Material Notes:
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.

Unfilled Extrusion Resins
Akulon resins are available with melt viscosities to suit all extrusion processes: barrier and coating film, tube and hose, monofilament, stock shapes. Akulon resins are characterized by:

  • consistent quality
  • high purity
  • for film applications, low gel contents.

Molding Resins
Suited to all engineering demands:

  • Unfilled low and medium viscosity grades
  • Toughened unfilled grades
  • Glass reinforced from 20-45% filled
  • Low warpage reinforced grades
  • Flame retardant; UL V0 rated and glow wire types
  • Halogen free FR grades
  • Blow moldable materials
  • Laser markable resins
  • Laser weldable, high burst pressure grades
  • Toughened, reinforced resins
  • High stiffness grades for metal replacement

Akulon Ultraflow resins have high flow with mechanical properties similar to standard materials. Exceptional flow allows:

  • productivity gains in molding
  • lower built in stresses
  • better surface appearance
  • system cost reductions

Applications for Molding resins There is an Akulon resin available suitable for any application requiring polyamides. Key areas where DSM has specific application knowledge are

  • Automotive
    • Under the hood and engine components
    • Exterior and interior applications
    • Electrical components and connectors
  • Electrical
    • Low voltage power distribution
    • Lighting
    • Power connectors
  • Consumer Durables
    • Power and lawn and garden tools
    • Small Appliances
    • Sports and leisure equipment
    • Furniture accessories
    • Industrial Goods
    • Transportation (railways)

Information provided by DSM.

Available Properties
  • Density
  • Water Absorption
  • Moisture Absorption at Equilibrium
  • Linear Mold Shrinkage
  • Linear Mold Shrinkage, Transverse
  • Tensile Strength at Break
  • Elongation at Break
  • Tensile Modulus
  • Charpy Impact Unnotched
  • Charpy Impact, Notched, Low Temp
  • Charpy Impact, Unnotched Low Temp
  • Charpy Impact, Notched
  • Volume Resistivity
  • Surface Resistance
  • Dielectric Constant
  • Dielectric Constant, Low Frequency
  • Dielectric Strength
  • Dissipation Factor
  • Dissipation Factor, Low Frequency
  • Melting Point
  • Injection Molding
  • Lubricants
  • Release agent
  • With fillers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。