DSM Arnitel® PM381 38 Shore D, Extrusion Grade Copolyester Elastomer (North America)
Subcategory: Elastomer, TPE; Thermoplastic; Polyester TPE
Material Notes: Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers. Arnitel does not require vulcanization. This leads to substantial reductions in part cost. Arnitel can be used over a wide range of temperatures. Arnitel has exceptional fatigue, creep resistance and resistance to oils, greases and many other chemicals. Characteristics of Arnitel: - Excellent strength over a wide range of temperatures
- Excellent dynamic properties e.g. creep and fatigue
- High heat resistance
- Exceptional resistance to oils and greases
- Good chemical resistance
- High degree of versatility in processing
- Easy coloring using masterbatches
- Surface quality from high gloss to textured
- Excellent heat resistance (long term 165°C)
- Good electrical insulation properties
- Low moisture absorption, excellent dimensional stability
- Easy flow, fast cooling times
Typical Applications: - Automotive: Arnitel® is extensively used in the automotive industry for applications requiring exceptional fatigue resistance and resistance to oil and greases. Examples are: Rack and Pinion Bellows, Constant Velocity Joint Boots (CVJ Boots), Air brake tubings.
- Arnitel in the Electronic and Consumer Goods Industry: Arnitel® finds enormous potential and is also widely used in the consumer electronics by some of the world's best companies. Arnitel® is the best choice for low noise gears where their exceptional processability without any defects such as flash, makes it the material solution of choice. Arnitel® is also used in highly demanding applications such as in mobile phone antennas.
Arnitel® has exceptional flexibility and can perform or even outperform functions that normally require conventional rubbers. Available in a wide range of hardnesses, Arnitel can replace metals, thermoplastics, leather and rubber, often with a reduction in finished part costs. Information provided by DSM.
| Available Properties |
- Density
- Water Absorption
- Moisture Absorption at Equilibrium
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Vicat Softening Point
- Flammability, UL94
- Film Extrusion
- High impact or impact modified
- Other Extrusion
- Profile Extrusion
- Sheet Extrusion
- Without fillers
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|