Nyrim® 1500, Conditioned
Subcategory: Nylon; Thermoplastic; Nylon 6
Key Words: Nylon others, polyamide 6, polyamide others, high impact nylon, RIM materials
Material Notes: Conditioned at 23°C and 50% Relative Humidity. Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark. Information provided by the manufacturer, Brueggemann Chemical.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Modulus of Elasticity
- Flexural Modulus
- Shear Modulus
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched (ISO)
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- Comparative Tracking Index
- Melting Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|