DuPont Delrin® 520MP NC010 Acetal (POM) Homopolymer
Subcategory: Acetal; Thermoplastic
Material Notes: Delrin® 520MP is a medium viscosity acetal homopolymer containing 20% Teflon® PTFE Micropowder. It is designed for applications requiring low wear and/or friction against steel, itself, and or other plastics.
| Available Properties |
- Density
- Specific Gravity
- Filler Content
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistance
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- CTE, linear 100°C
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- Drying
- DuPont Product Category
- Extrudable
- Features
- Form
- Injection Moldable
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Ultrasonic Weldable
- Uses
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|