DuPont Hytrel® G3548L TPC-ET
Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic
Material Notes: Hytrel® G3548L is a low modulus grade with nominal hardness of 35D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection molding and extrusion.
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Linear Mold Shrinkage, Transverse
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched, Low Temp (ISO)
- Charpy Impact, Notched, Low Temp
- Izod Impact, Notched
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Melting Point
- Brittleness Temperature
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- Drying
- DuPont Product Category
- Extrudable
- Extrusion Blow Moldable
- Features
- Form
- Heat Stabilized
- Injection Blow Moldable
- Injection Moldable
- Melt Castable
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Uses
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|