DuPont Hytrel® HTR6108 TPC-ET
Subcategory: Polyester, TP; Elastomer, TPE; Thermoplastic
Material Notes: Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various thermoplastic processing techniques.
| Available Properties |
- Density
- Specific Gravity
- Water Absorption
- Melt Flow
- Hardness, Shore D
- Tensile Strength at Break
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Brittleness Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Additive
- Appearance
- Drying
- DuPont Product Category
- Extrudable
- Features
- Form
- Heat Stabilized
- Injection Moldable
- Melt Castable
- Part Marking Code
- Processing Method
- Region
- Resin Identification
- Uses
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|